这里是标题一h1占位文字
The solution to the residual glue of BOPP protective film
Release time:
2025-12-16
In the process of daily use, we can find that some oPP protective films have residual pressure-sensitive adhesive on the protected surface in use, and it is not easy to remove.
In the process of daily use, we can find that some oPP protective films have residual pressure-sensitive adhesive on the protected surface in use, and it is not easy to remove. Therefore, this problem has to make the production and use of protective film the most difficult glue residue problem for manufacturers, which not only affects the appearance, but also causes material pollution. So why does the OPP protective film have such a problem? What is the reason? Let me tell you about it below.
There are usually three situations in the residual adhesive of OPP protective film. First, cohesive damage: there are pressure-sensitive adhesives on the protected surface and the substrate, and the coated surface of the protective film loses its luster; second, the adhesive base is damaged: the protected surface There is a lot of glue residue, and the base material is visible on the glued surface of the protective film. Third, migration residues: There is a small amount of pressure-sensitive glue residue on the protected surface, and the gloss of the glued surface of the protective film remains good.

One of the more common reasons is that the peel strength of the OPP protective film has changed after a period of time. After the protective film is attached to the protective material, it will take a period of time to remove the protective film. The short time is only a few minutes, and the long one is one year. Most of the above are within 3 to 12 months. During this period, the peel strength of the protective film tends to increase with the continuation of time, usually first fast and then slow, and finally tends to be stable. When the peel strength rises above the cohesive strength or adhesive base force, cohesive failure or adhesive base failure occurs, resulting in adhesive residue.
Another reason is the aging of the OPP protective film. The protective film is composed of a plastic substrate and a pressure-sensitive adhesive, both of which are high molecular polymers. The aging mechanisms mainly include thermal aging and ultraviolet light aging. After the protective film is aged, the macromolecular chains constituting the substrate and the pressure-sensitive adhesive are broken, the average molecular weight is reduced, and the cohesive strength is reduced, and then cohesive failure occurs.
Other News
You can also learn more dynamic
2025/12/16
Hongyan once again appears on CCTV: Private enterprise innovation 'landing into gold', government builds' technology golden bridge '
2025/12/16
Application and use of PET protective film of different thickness
With the popularization and application of protective film, smart product decorations such as screen protective film and pet protective film have also developed rapidly, especially the pet protective film has attracted more attention.
2025/12/16
The solution to the residual glue of BOPP protective film
In the process of daily use, we can find that some oPP protective films have residual pressure-sensitive adhesive on the protected surface in use, and it is not easy to remove.
2025/12/16
How to control the transparency of PE protective film?
Due to blowing and stretching, the molecular orientation is serious, resulting in low elongation at break; while the casting production has good cooling effect, low crystallinity, good transparency, and low degree of orientation, so the elongation at break is high and retractable.